Grinding Wheel FAQ: Diamond, CBN, Bonds, Grit, Speed and Safety

Assorted diamond and CBN grinding wheels
The FAQ hub links common questions to the detailed selection, dressing and application guides.

Quick answer: This FAQ hub answers the questions engineers ask most often about diamond and CBN grinding: which abrasive, which bond, which grit, how fast, whether to use coolant, how to dress and how to compare cost. Each answer links to the detailed guide or tool that covers it.

Start with the right cluster

Applications

Cost and ordering

Boundary rule — when not to use diamond

Diamond is the hardest abrasive and the correct choice for hard, brittle, non-ferrous materials such as cemented carbide, ceramics, glass, silicon, sapphire, ferrite, graphite and composites. It must not be used on ferrous metals — steel, cast iron, and their alloys — because carbon in diamond reacts with iron at grinding temperatures (roughly above 700 °C / 1300 °F). This chemical affinity causes rapid, abnormal diamond wear (graphitisation) and destroys the wheel. For steel, hardened steel, cast iron and other ferrous workpieces, use CBN (cubic boron nitride) instead.

Next steps

Related application guides

Shop-floor verification checklist

Before releasing a grinding process to production, verify the basics on the machine. Small errors in speed, balance, coolant or dressing often show up as burn, chatter or inconsistent finish after a few parts.

Common mistakes to avoid

Standards and verification references

The wheel marking, machine data and applicable standards are the baseline for every setup. Typical references include ISO 6106 for superabrasive grit size, FEPA 61 for diamond and CBN grit designations, and EN 13218 / ANSI B7.1 for machine safety and wheel speed limits.

Key takeaways for buyers & engineers

Quick selection checklist

Need a custom specification? Send your drawing or current wheel marking and we will quote a diamond wheel to fit your material, machine and finish target — OEM, custom and private label supported.

Frequently Asked Questions

Should I use diamond or CBN?

Use diamond for hard, brittle, non-ferrous materials such as carbide, ceramics, glass and composites. Use CBN for steel, cast iron and other ferrous metals.

Can diamond grind steel?

No. Diamond reacts with iron at grinding temperature and wears abnormally. Use CBN for steel and cast iron.

How do I choose a grinding wheel grit?

Start with the finish and stock removal. Coarser grit removes material faster; finer grit gives a lower Ra. For diamond, use FEPA D sizes such as D126 for general work and D46 for fine finishing.

What does diamond concentration mean?

Concentration is the amount of diamond in the bond. 100 is the standard reference (4.4 carat per cm3, i.e. 0.88 g/cm3). Higher concentration generally gives longer life and better form retention.

Which bond should I choose?

Resin for cool cutting and fine finish, metal for life and form, vitrified for free cutting and profile control, electroplated for small or complex tools.

What wheel speed should I use?

Set surface speed in m/s, not a fixed RPM. Common ranges are 20-35 m/s for diamond and 25-40 m/s for vitrified CBN; always check the wheel marking.

Do I need coolant?

Wet grinding is preferred for heat-sensitive steels, CBN, vitrified wheels and high removal rates. Light resin-bond diamond finishing can run dry with dust extraction.

How often should I dress a wheel?

Dress when the wheel glazes, loads, burns, loses form or the finish deteriorates. There is no fixed interval; monitor power, finish and spark colour.

What is the difference between truing and dressing?

Truing restores geometry such as roundness and profile; dressing restores sharpness by exposing fresh grit.

Why is my wheel glazing?

Glazing is caused by a bond that is too hard, a wheel that is too fine, excessive wheel speed or too light a depth of cut. Open the bond, increase the depth of cut or feed, or dress more often.

Why is my wheel loading?

Loading is workpiece material sticking to the wheel. It is common on aluminium, soft steels and composites; use a coarser, more open wheel and better coolant.

Does wheel balancing affect finish?

Yes. Imbalance causes chatter and vibration, which show up as periodic marks and poor Ra. Balance after mounting and dressing.

How can I make a wheel last longer?

Use the correct bond and grit, control coolant, avoid excessive depth of cut, dress correctly and keep the machine rigid.

What is G-ratio?

G-ratio is the volume of workpiece removed divided by the volume of wheel worn. A higher G-ratio means more efficient wheel use.

Which wheel for carbide?

Diamond is the usual choice. Resin bond for tool-room finishing and vitrified or metal bond for form and production work.

Which wheel for hardened steel?

CBN, usually in a vitrified or resin bond, is the first choice for hardened steel above about 45 HRC.

Which wheel for aluminium?

Silicon carbide with a coarse, open structure and flood coolant is the usual choice. Diamond can be used on high-silicon aluminium with care.

Which wheel for glass or ceramics?

Diamond, usually metal or vitrified bond, selected for edge quality and form retention.

Which wheel for PCD or PCBN?

Diamond wheels in resin or vitrified bond are used for edge preparation and fine grinding of PCD and PCBN.

Which wheel for stone?

Diamond segments in a metal bond for granite, marble and engineered stone; choose grit by finish and machine power.

What coolant should I use?

A clean water-based emulsion suits most ferrous and CBN grinding. Neat oil is used in some precision processes. Control concentration, flow and filtration.

What safety checks before mounting a wheel?

Check for cracks and damage, confirm the maximum speed, use the correct flanges and guard, and stand clear when starting.

How should I store grinding wheels?

Store in a dry, frost-free place, on a flat surface, away from impact and solvents. Do not stack heavy wheels on thin ones.

Why is diamond wheel price so variable?

Price depends on abrasive, grit, concentration, bond, size and shape, tolerance, substrate, testing and order quantity. Compare cost per part, not just wheel price.

Can I order a custom diamond or CBN wheel?

Yes. Provide a drawing or specification with dimensions, bond, grit, concentration, workpiece, machine and quantity so the supplier can quote accurately.